ASA density and cost per gram
ASA density runs from 1.05 to 1.13 g/cm³ across makers' datasheets. The price per gram from their stores, and the plastic in a 480 g fixture.
Density, by datasheet
| ASABambu Lab TDS | 1.05 g/cm³ · 396 m per kg |
| ASAElegoo | 1.09 g/cm³ · 381 m per kg |
| Polymaker ASAPolymaker | 1.13 g/cm³ · 368 m per kg |
Metres per kilogram of 1.75 mm filament, worked out from each density: a denser plastic puts fewer metres on the same kilogram, so a slicer that reports length needs the density of the roll you load.
Price per gram, by maker
| ASA, $29.99 for 1000 gBambu Lab store | $0.0300 a gram |
| Prusament ASA, $27.99 for 800 gPrusa store | $0.0350 a gram |
| ASA, $16.99 for 1000 gElegoo | $0.0170 a gram |
List prices on each maker’s US store, without a sale, on the day in the sources. Type your own in the filament cost calculator.
What fixture plate costs in plastic
480 g of model and 10 g of purge and supports, both charged at the spool’s price per gram.
| ASA | $14.70 |
| Prusament ASA | $17.14 |
| ASA | $8.33 |
The plastic is one line of a quote. Power, machine hours, your time and failed prints are the rest, and the cost calculator prices them all.
From the ASA datasheets
- Bambu Lab's ASA datasheet asks for a 45 to 60 °C chamber while it prints, and rates the material at 100 °C of heat deflection under 0.45 MPa.Bambu Lab TDS
- Prusa Polymers recommends a skirt or an enclosure for Prusament ASA, with the bed at 110 °C and the nozzle at 260 °C.Prusament
- A Prusament ASA spool holds 800 g, not a kilogram, so its price per gram is higher than its shelf price suggests.Prusa store
Compare ASA
- ABS vs ASA: strength, heat and costABS starts to bend under load at 87 °C and ASA at 100 °C. Compare strength, print settings, drying and price per gram from Bambu Lab's datasheets.
- ASA vs PETG: strength, heat and costASA starts to bend under load at 100 °C and PETG at 71 °C. Compare strength, print settings, drying and price per gram from Bambu Lab's datasheets.
Other materials
Keep these numbers for every print
Printyard runs this arithmetic on your phone at the machine and on the web: every quote itemised, every roll to the gram, and a month with the fees and the failed prints already taken out.
Sources
- ASA technical data sheet V3.0 · Bambu Lab · checked November 5, 2026
- ELEGOO ASA filament 1.75 mm, 1 kg: $16.99 and the material's specifications · Elegoo · checked October 30, 2026
- Polymaker ASA technical data sheet · Polymaker · checked November 5, 2026
- ASA, 1 kg: typical price $29.99, shown beside a $17.99 sale price · Bambu Lab US Store · checked October 30, 2026
- Prusament ASA Jet Black 800 g: regular price $27.99, shown beside a $22.99 sale price · Prusa Research · checked October 30, 2026
- Prusament ASA: material page and printer requirements · Prusa Polymers · checked October 30, 2026