TPU density and cost per gram
TPU 95A density from Bambu Lab and Elegoo, the price per gram from their stores, and what a 30 g phone case costs in flexible filament.
Density, by datasheet
| TPU 95A HFBambu Lab TDS | 1.22 g/cm³ · 341 m per kg |
| TPU 95AElegoo | 1.16 g/cm³ · 358 m per kg |
Metres per kilogram of 1.75 mm filament, worked out from each density: a denser plastic puts fewer metres on the same kilogram, so a slicer that reports length needs the density of the roll you load.
Price per gram, by maker
| TPU 95A HF, $41.99 for 1000 gBambu Lab store | $0.0420 a gram |
| TPU 95A, $17.99 for 1000 gElegoo | $0.0180 a gram |
List prices on each maker’s US store, without a sale, on the day in the sources. Type your own in the filament cost calculator.
What phone case costs in plastic
30 g of model and 2 g of purge and supports, both charged at the spool’s price per gram.
| TPU 95A HF | $1.34 |
| TPU 95A | $0.58 |
The plastic is one line of a quote. Power, machine hours, your time and failed prints are the rest, and the cost calculator prices them all.
From the TPU datasheets
- Bambu Lab's TPU 95A HF stretches more than 650% before it breaks, by its datasheet.Bambu Lab TDS
- Elegoo states its empty TPU spool weighs 165 ± 5 g, the figure to subtract when you weigh a roll on a kitchen scale.Elegoo
Other materials
Keep these numbers for every print
Printyard runs this arithmetic on your phone at the machine and on the web: every quote itemised, every roll to the gram, and a month with the fees and the failed prints already taken out.
Sources
- TPU 95A HF technical data sheet · Bambu Lab · checked November 5, 2026
- ELEGOO TPU filament 1.75 mm, 1 kg: $17.99 and the material's specifications · Elegoo · checked October 30, 2026
- TPU 95A HF, 1 kg with spool: typical price $41.99, shown beside a $25.19 sale price · Bambu Lab US Store · checked October 30, 2026